No title
In-situ, time-resolved small-angle neutron scattering (SANS) investigations of the early stages of the spinodal decomposition process in Fe-35Cr were performed at 773 and 798K. The kinetics of the decomposition, both in terms of characteristic distance and peak intensity, followed a power-law behaviour from the start of the heat treatment (a' = 0.10-0.11 and a '' = 0.67-0.86). Furthermore, the met